Lead-Free (K0.5Na0.5)NbO3 Unmodified Piezoceramics: A Reduction in the Energetic Budget of Solid State Synthesis and Sintering

Articolo
Data di Pubblicazione:
2025
Citazione:
Lead-Free (K0.5Na0.5)NbO3 Unmodified Piezoceramics: A Reduction in the Energetic Budget of Solid State Synthesis and Sintering / Dore, Maria; Bartolomé José, F.; Lopez-Esteban, Sonia; Mureddu, Marzia; Cau, Costantino; Enzo, Stefano; García, Álvaro; Garroni, Sebastiano; Lorena, Pardo. - In: CHEMISTRY METHODS. - ISSN 2628-9725. - (2025). [10.1002/cmtd.202500038]
Abstract:
Replacement of the ubiquitous lead titanate zirconate piezoceramics is still a challenge involving sustainable materials and processes. An extended effort has been paid for the optimization of the properties of (K0.5Na0.5)NbO3 (KNN) lead-free piezoceramics at the expenses of high-energetic budget. A sustainable solid-state processing with potential for industrial scaling (knowledge-based, sustainable, reproducible, and cost-effective) is still lacking. In this work, an efficient solution is proposed using the well-known and noncontaminant attrition-ball-milling of the mixture of reagents for only 3 h, prior to the synthesis tests at increasing temperatures. After calcination at only 450 °C/2 h, 60 wt% KNN is achieved. Moreover, after 850 °C/2 h the calcined powder becomes a pure KNN. A second ball-milling of powder calcined at 700850 °C gives place to populations of nanostructured particles (380–40 nm, respectively). The milled powder calcined at 700 °C is pressureless sintered in air for 2 h at 1050 and 1100 °C, leading to coarse grained ceramics. Milled powder calcined at 750 and 850 °C, sintered at the same conditions, produces fine grain homogeneous microstructures. Ceramics show an orthorhombic Amm2 pure KNN perovskite phase, as seen by x-ray diffraction and Rietveld analysis. The piezoelectric values (d33 = 115 pC/N, d31 = −22 pC/N, kp = 20%, kt = 40%) are exceptional when derived from such a straightforward solid-state route.
Tipologia CRIS:
1.1 Articolo in rivista
Elenco autori:
Dore, Maria; Bartolomé José, F.; Lopez-Esteban, Sonia; Mureddu, Marzia; Cau, Costantino; Enzo, Stefano; García, Álvaro; Garroni, Sebastiano; Lorena, Pardo
Autori di Ateneo:
ENZO Stefano
GARRONI Sebastiano
Link alla scheda completa:
https://iris.uniss.it/handle/11388/373249
Pubblicato in:
CHEMISTRY METHODS
Journal
  • Dati Generali

Dati Generali

URL

https://chemistry-europe.onlinelibrary.wiley.com/doi/full/10.1002/cmtd.202500038
  • Utilizzo dei cookie

Realizzato con VIVO | Designed by Cineca | 26.7.0.0